This file is automatically generated. It contains the descriptions of each uploaded file as provided by the user.
- Figure 1.zip: OER performance of Ni-MOF-74 and its Fe uptake from Fe-containing 0.1 M KOH
- Figure 2.zip: Ex situ XRD and operando hXAS measurements of Ni-MOF-74 in Fe-free and 5 ppm Fe contaminated 0.1 M KOH electrolyte
- Figure 3.zip: Activity and Stability of Ni-MOC* upon Fe incorporation from Fe-containing 0.1 M KOH electrolyte
- Figure 4.zip: Operando hXAS measurements of Ni K edge of Ni-MOC* during OER in clean and 5 ppm Fe contaminated 0.1 M KOH
- Figure 5.zip: Performance of Ni-MOC* anode in AEM-WE in Fe-free and 3 ppm Fe contaminated 1 M KOH